Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP PI001 PA 6 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP PI001 PA 6 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* PI001 is a compound based on PA 6 resin containing Silicone. Added features include Internally Lubricated.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 43.0 MPa
6240 psi
50 mm/min; ISO 527
Tensile Strength, Yield 70.0 MPa
10200 psi
50 mm/min; ISO 527
Elongation at Break 6.6 %
6.6 %
50 mm/min; ISO 527
Tensile Modulus 2.50 GPa
363 ksi
1 mm/min; ISO 527
Flexural Yield Strength 82.0 MPa
11900 psi
2 mm/min; ISO 178
Flexural Modulus 2.10 GPa
305 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 125 kJ/m²
59.5 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 116 µm/m-°C

@Temperature 23.0 - 60.0 °C
64.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature 23.0 - 60.0 °C
65.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 153 °C
307 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 53.0 °C
127 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af