Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP PFI12R PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP PFI12R PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* PFI12R is a compound based on Nylon 6 resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Mold Release.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 cm/cm

@Time 86400 sec
0.0050 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 105 MPa
15200 psi
ASTM D638
Elongation at Break 3.2 %
3.2 %
ASTM D638
Tensile Modulus 4.95 GPa
718 ksi
50 mm/min; ASTM D638
Flexural Strength 151 MPa
21900 psi
ASTM D790
Flexural Modulus 5.25 GPa
761 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.13 J/cm
13.4 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 202 °C

@Thickness 3.20 mm
396 °F

@Thickness 0.126 in
unannealed; ASTM D648