SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 MPa
6670 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Tensile Modulus 2.68 GPa
389 ksi
50 mm/min; ASTM D638
Flexural Strength 82.0 MPa
11900 psi
ASTM D790
Flexural Modulus 2.79 GPa
405 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C

@Thickness 3.20 mm
205 °F

@Thickness 0.126 in
unannealed; ASTM D648