SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.00050 - 0.0025 cm/cm
0.00050 - 0.0025 in/in
on Tensile Bar; SABIC Method
Melt Index of Compound 50 g/10 min

@Load 5.00 kg,
Temperature 315 °C
50 g/10 min

@Load 11.0 lb,
Temperature 599 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 157 MPa
22800 psi
5 mm/min; ISO 527
Elongation at Break 1.5 %
1.5 %
5 mm/min; ISO 527
Tensile Modulus 12.6 GPa
1830 ksi
1 mm/min; ISO 527
Flexural Strength 212 MPa
30700 psi
2 mm/min; ISO 178
Flexural Modulus 11.1 GPa
1610 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 25.0 kJ/m²
11.9 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 14.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
7.78 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 52.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
28.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 243 °C
469 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257