SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP (Asia Pacific)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE. Added features of this material include: Internally Lubricated, Heat Stabilized, Low Extractible.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 32 %
32 %
ASTM D638
Tensile Modulus 1.58 GPa
229 ksi
50 mm/min; ASTM D638
Flexural Strength 34.0 MPa
4930 psi
ASTM D790
Flexural Modulus 1.37 GPa
199 ksi
ASTM D790
Izod Impact, Notched 0.210 J/cm
0.393 ft-lb/in
ASTM D256
Izod Impact, Unnotched 3.20 J/cm
5.99 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C

@Thickness 3.20 mm
144 °F

@Thickness 0.126 in
unannealed; ASTM D648