SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
5 mm/min; ISO 527
Elongation at Break 2.8 %
2.8 %
5 mm/min; ISO 527
Tensile Modulus 6.90 GPa
1000 ksi
1 mm/min; ISO 527
Flexural Strength 123 MPa
17800 psi
2 mm/min; ISO 178
Flexural Modulus 6.40 GPa
928 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 50.0 kJ/m²
23.8 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
16.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 117 µm/m-°C

@Temperature 23.0 - 60.0 °C
65.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2