SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* KP004AXZ is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D792
1.49 g/cc
0.0538 lb/in³
ISO 1183
Moisture Absorption 0.200 %
0.200 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.021 cm/cm

@Time 86400 sec
0.021 in/in

@Time 24.0 hour
ASTM D955
0.0214 cm/cm

@Time 86400 sec
0.0214 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0205 cm/cm

@Time 86400 sec
0.0205 in/in

@Time 24.0 hour
ISO 294
0.021 cm/cm

@Time 86400 sec
0.021 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ISO 527
50.0 MPa
7250 psi
ASTM D638
Elongation at Break 10.5 %
10.5 %
ISO 527
12.5 %
12.5 %
ASTM D638
Tensile Modulus 2.20 GPa
319 ksi
50 mm/min; ASTM D638
2.60 GPa
377 ksi
1 mm/min; ISO 527
Flexural Strength 75.0 MPa
10900 psi
ASTM D790
77.0 MPa
11200 psi
ISO 178
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
2.80 GPa
406 ksi
ISO 178
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.27 J/cm
8.00 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 5.00 J
3.69 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 1.00 J
0.738 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.25
0.25
ASTM D3702 Modified
Coefficient of Friction, Static 0.16
0.16
ASTM D3702 Modified
K (wear) Factor 18.1 x 10-8 mm³/N-M
9.00 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 163 °C

@Thickness 3.20 mm
325 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
99.0 °C

@Thickness 3.20 mm
210 °F

@Thickness 0.126 in
unannealed; ASTM D648