Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP IP004Z PA6.12 (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP IP004Z PA6.12 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* IP004Z is a compound based on PA 6/12 resin containing PTFE, Silicone. Added features include : Internally Lubricated, Extrusion grade.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ISO 1183
Water Absorption 0.35 %

@Time 86400 sec
0.35 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.021 cm/cm
0.021 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 47.0 MPa
6820 psi
50 mm/min; ISO 527
Elongation at Yield 13.8 %
13.8 %
50 mm/min; ISO 527
Tensile Modulus 1.90 GPa
276 ksi
1 mm/min; ISO 527
Flexural Yield Strength 60.0 MPa
8700 psi
2 mm/min; ISO 178
Flexural Modulus 1.80 GPa
261 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 4.00 kJ/m²
1.90 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 55.0 kJ/m²
26.2 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 127 µm/m-°C

@Temperature 23.0 - 60.0 °C
70.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 122 µm/m-°C

@Temperature 23.0 - 60.0 °C
67.8 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
289 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °C
142 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Copyright © lookpolymers.com All Rights Reserved