Material Notes:
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing PTFE. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.020 cm/cm

@Time 86400 sec
0.020 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D638
Elongation at Break 42 %
42 %
ASTM D638
Tensile Modulus 1.43 GPa
207 ksi
50 mm/min; ASTM D638
Flexural Strength 20.0 MPa
2900 psi
ASTM D790
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 0.260 J/cm
0.487 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C

@Thickness 3.20 mm
115 °F

@Thickness 0.126 in
unannealed; ASTM D648