Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DZL24 PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* DZL24 is a compound based on Polycarbonate resin containing PTFE, Milled Glass. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 37.0 MPa
5370 psi
ASTM D638
Elongation at Break 28 %
28 %
ASTM D638
Tensile Modulus 0.300 GPa
43.5 ksi
50 mm/min; ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.21 J/cm
21.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C

@Thickness 3.20 mm
270 °F

@Thickness 0.126 in
unannealed; ASTM D648
Copyright © lookpolymers.com All Rights Reserved