Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* LUBRICOMP* DL0039E is a compound based on Polycarbonate resin containing PTFE, Flame retardant. Added features include: Easy Molding, Internally Lubricated, Flame retardant.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 53.0 MPa
7690 psi
5 mm/min; ISO 527
Elongation at Yield 4.8 %
4.8 %
5 mm/min; ISO 527
Tensile Modulus 2.30 GPa
334 ksi
1 mm/min; ISO 527
Flexural Yield Strength 89.0 MPa
12900 psi
2 mm/min; ISO 178
Flexural Modulus 2.30 GPa
334 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 8.00 kJ/m²
3.81 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 60.0 kJ/m²
28.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 73.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
40.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 71.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
39.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 131 °C
268 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
UL 94 by SABIC-IP
Users viewing this material also viewed the following: