Material Notes:
LNP* LUBRICOMP* DFP36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Moisture Absorption 0.0800 %
0.0800 %
50% RH, 24 hrs; ASTM D570
0.120 %
0.120 %
23°C / 50% RH; ISO 62
Mechanical Properties Metric English Comments
Tensile Modulus 8.70 GPa
1260 ksi
1 mm/min; ISO 527
Izod Impact, Notched 1.79 J/cm
3.35 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.36 J/cm
13.8 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 16.0 kJ/m²
7.61 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 49.0 kJ/m²
23.3 ft-lb/in²
80*10*4; ISO 180/1U
Impact Test 7.00 J
5.16 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C

@Thickness 3.20 mm
295 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 144 °C
291 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af