Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC (Asia Pacific)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP DFL28EG PC (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* DFL28EG is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 124 MPa
18000 psi
ASTM D638
Elongation at Break 2.1 %
2.1 %
ASTM D638
Tensile Modulus 11.03 GPa
1600 ksi
50 mm/min; ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 10.54 GPa
1529 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.40 J/cm
12.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 140 °C

@Thickness 3.20 mm
284 °F

@Thickness 0.126 in
unannealed; ASTM D648