Material Notes:
LNP* Lubricomp* DFL16E is a compound based on Polycarbonate resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated, Easy Molding.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Tensile Modulus 8.81 GPa
1280 ksi
50 mm/min; ASTM D638
Flexural Strength 151 MPa
21900 psi
ASTM D790
Flexural Modulus 7.92 GPa
1150 ksi
ASTM D790
Izod Impact, Notched 0.900 J/cm
1.69 ft-lb/in
ASTM D256
Izod Impact, Unnotched 6.55 J/cm
12.3 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 140 °C

@Thickness 3.20 mm
284 °F

@Thickness 0.126 in
unannealed; ASTM D648