Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP CX05031 PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* CX05031 is a compound based on Polystyrene resin containing Graphite, Silicone. Added features include; Internally Lubricated.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.0 MPa
3480 psi
5 mm/min; ISO 527
Tensile Strength, Yield 30.0 MPa
4350 psi
5 mm/min; ISO 527
Elongation at Break 2.4 %
2.4 %
Flexural Strain, break, 2 mm/min; ISO 178
Elongation at Yield 0.60 %
0.60 %
5 mm/min; ISO 527
Tensile Modulus 6.90 GPa
1000 ksi
1 mm/min; ISO 527
Flexural Strength 48.0 MPa
6960 psi
2 mm/min; ISO 178
Flexural Yield Strength 51.0 MPa
7400 psi
2 mm/min; ISO 178
Flexural Modulus 6.40 GPa
928 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 3.00 kJ/m²
1.43 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 81.0 °C
178 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af