Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP LUBRICOMP CGI11XP PS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP CGI11XP PS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* CGI11XP is a compound based on Polystyrene resin containing Graphite. Added features include: Internally Lubricated.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 MPa
6670 psi
5 mm/min; ISO 527
Elongation at Break 2.7 %
2.7 %
5 mm/min; ISO 527
Tensile Modulus 3.30 GPa
479 ksi
1 mm/min; ISO 527
Flexural Modulus 3.10 GPa
450 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 2.00 kJ/m²
0.952 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af