SABIC Innovative Plastics LNP Faradex NS0029 PC+ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Antistat/Conductive , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Faradex NS0029 PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* NS0029 is a compound based on PC+ABS Blend resin containing Flame Retardant, Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding, Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 61.0 MPa
8850 psi
5 mm/min; ISO 527
Elongation at Break 7.8 %
7.8 %
5 mm/min; ISO 527
Flexural Strength 99.0 MPa
14400 psi
2 mm/min; ISO 178
Flexural Modulus 3.20 GPa
464 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²

@Temperature 23.0 °C
2.86 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 2.00 mm
V-0

@Thickness 0.0787 in
UL 94
Electrical Properties Metric English Comments
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D 257