SABIC Innovative Plastics LNP FARADEX AS004 ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP FARADEX
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP FARADEX AS004 ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Faradex* AS004 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.0 MPa
6380 psi
5 mm/min; ISO 527
Elongation at Yield 2.1 %
2.1 %
5 mm/min; ISO 527
Tensile Modulus 3.40 GPa
493 ksi
1 mm/min; ISO 527
Flexural Strength 60.0 MPa
8700 psi
2 mm/min; ISO 178
Flexural Modulus 3.10 GPa
450 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 15.0 kJ/m²
7.14 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 10 - 1000 ohm
10 - 1000 ohm
ASTM D257