Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP COLORCOMP J1000Z PES (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP J1000Z PES (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* COLORCOMP* is a compound based on Polyethersulfone resin. Added features include: High Viscosity
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ISO 1183
Water Absorption 1.8 %

@Time 86400 sec
1.8 %

@Time 24.0 hour
ISO 62-1
Linear Mold Shrinkage, Flow 0.010 cm/cm
0.010 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 72.0 MPa
10400 psi
50 mm/min; ISO 527
Tensile Strength, Yield 89.0 MPa
12900 psi
50 mm/min; ISO 527
Elongation at Yield 6.9 %
6.9 %
50 mm/min; ISO 527
Tensile Modulus 2.60 GPa
377 ksi
1 mm/min; ISO 527
Flexural Yield Strength 130 MPa
18900 psi
2 mm/min; ISO 178
Flexural Modulus 2.80 GPa
406 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
NB
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 206 °C
403 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af