SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Colorcomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
1.16 g/cc
0.0419 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ISO 294
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ASTM D955
0.0050 - 0.0070 cm/cm

@Time 86400 sec
0.0050 - 0.0070 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
31.0 MPa
4500 psi
ISO 527
Tensile Strength, Yield 38.0 MPa
5510 psi
ISO 527
39.0 MPa
5660 psi
ASTM D638
Elongation at Break 13.6 %
13.6 %
ASTM D638
15.3 %
15.3 %
ISO 527
Elongation at Yield 2.0 %
2.0 %
ISO 527
2.1 %
2.1 %
ASTM D638
Tensile Modulus 2.39 GPa
347 ksi
1 mm/min; ISO 527
2.44 GPa
354 ksi
50 mm/min; ASTM D638
Flexural Strength 65.0 MPa
9430 psi
ASTM D790
65.0 MPa
9430 psi
ISO 178
Flexural Modulus 2.31 GPa
335 ksi
ISO 178
2.39 GPa
347 ksi
ASTM D790
Izod Impact, Notched 1.70 J/cm
3.18 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.68 J/cm
20.01 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²
5.23 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 39.0 kJ/m²
18.6 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
72.0 °C

@Thickness 3.20 mm
162 °F

@Thickness 0.126 in
unannealed; ASTM D648