Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Geloy INP983 ASA

Category Polymer , Thermoplastic , ASA Polymer , Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name GELOY
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Geloy INP983 ASA.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SABIC INP983 is a 32% polybutyl acrylate rubber grafted weatherable ASA modifier resin. Provides excellent impact, heat distortion and weatherability properties. Maintains polymer properties in UV and thermal environments. Toughens compatible rigid polymers without additional impact modification. Expands the use temperature window of compounds. Offers compatibility with many polar polymers.Improve UV resistance when blend with less stable polymers.SABIC INP983 is well suited to produce good weatherability in rigid polymer applications. Can be effectively alloyed with PVC and other miscible thermoplastics in molded, extruded or calendered applications to provide improved heat distortion and impact strength.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
ASTM D 792
Density 1.07 g/cc
0.0387 lb/in³
molded; ISO 1183
Volatiles 0.20 %
0.20 %
Total NA Volatiles; SABIC Method
Particle Size 250 µm
250 µm
mean resin; SABIC Method
Mechanical Properties Metric English Comments
Hardness, Shore D 73
73
ASTM D 2240
Descriptive Properties Value Comments
Rubber, % 32
SABIC Method