Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Enduran 7062X PBT+PET (Asia Pacific)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polyethylene Terephthalate (PET)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Enduran
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Enduran 7062X PBT+PET (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This data was supplied by SABIC-IP for the Asia Pacific region.
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
ASTM D 792
Water Absorption 0.070 %

@Time 86400 sec
0.070 %

@Time 24.0 hour
ASTM D 570
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0050 in/in

@Thickness 0.126 in
SABIC Method
0.0080 - 0.013 cm/cm

@Thickness 6.40 mm
0.0080 - 0.013 in/in

@Thickness 0.252 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 132 MPa
19100 psi
SABIC - Japan Method
Elongation at Break 10 %
10 %
SABIC - Japan Method
Flexural Strength 162 MPa
23500 psi
ASTM D 790
Flexural Modulus 10.14 GPa
1471 ksi
ASTM D 790
Izod Impact, Notched 0.420 J/cm

@Temperature 23.0 °C
0.787 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 4.31 J/cm

@Temperature 23.0 °C
8.07 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
Thermal Properties Metric English Comments
CTE, linear 30.0 - 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
16.7 - 44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 205 °C

@Thickness 3.20 mm
401 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 218 °C

@Thickness 3.20 mm
424 °F

@Thickness 0.126 in
unannealed; ASTM D 648