Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® CY4000 PC+ABS (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® CY4000 PC+ABS (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cycoloy* CY4000 resin is an injection moldable, flame retardant PC/ABS blend free of brominated or chlorinated flame resistant additives. Cycoloy CY4000 has excellent flow and balanced impact properties and is available for various color options. It is an ideal candidate for a wide variety of different applications.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
on Tensile Bar; SABIC Method
Melt Flow 23 g/10 min

@Load 2.16 kg,
Temperature 260 °C
23 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
Melt Index of Compound 21 g/10 min

@Load 2.16 kg,
Temperature 260 °C
21 g/10 min

@Load 4.76 lb,
Temperature 500 °F
MVR [cm^3/10 min]; ISO 1133
Mechanical Properties Metric English Comments
Hardness, H358/30 110 MPa
16000 psi
ISO 2039-1
Tensile Strength at Break 45.0 MPa
6530 psi
50 mm/min; ISO 527
Tensile Strength, Yield 55.0 MPa
7980 psi
50 mm/min; ISO 527
Elongation at Break >= 40 %
>= 40 %
50 mm/min; ISO 527
Elongation at Yield 3.0 %
3.0 %
50 mm/min; ISO 527
Tensile Modulus 2.70 GPa
392 ksi
1 mm/min; ISO 527
Flexural Yield Strength 85.0 MPa
12300 psi
2 mm/min; ISO 178
Flexural Modulus 2.50 GPa
363 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*3; ISO 180/1A
10.0 kJ/m²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
80*10*3; ISO 180/1A
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
Edgew 80*10*3 sp=62mm; ISO 179/1eA
1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Taber Abrasion, mg/1000 Cycles 15
15
CS-17, 1 kg; SABIC Method
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
Edgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
162 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 85.0 °C
185 °F
Rate B/50; ISO 306
90.0 °C
194 °F
Rate B/120; ISO 306
UL RTI, Electrical 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical with Impact 60.0 °C
140 °F
UL 746B
UL RTI, Mechanical without Impact 60.0 °C
140 °F
UL 746B
Flammability, UL94 V-0

@Thickness 2.50 mm
V-0

@Thickness 0.0984 in
UL 94 by SABIC-IP
Oxygen Index 29 %
29 %
ISO 4589
Glow Wire Test 960 °C

@Thickness 3.20 mm
1760 °F

@Thickness 0.126 in
IEC 60695-2-12
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
IEC 60093
Surface Resistance >= 1.00e+15 ohm
>= 1.00e+15 ohm
ROA; IEC 60093
Dielectric Constant 2.7

@Frequency 1.00e+6 Hz
2.7

@Frequency 1.00e+6 Hz
IEC 60250
2.7

@Frequency 50.0 - 60.0 Hz
2.7

@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm

@Thickness 3.20 mm
432 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
Dissipation Factor 0.0060

@Frequency 50.0 - 60.0 Hz
0.0060

@Frequency 50.0 - 60.0 Hz
IEC 60250
0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 600 V
600 V
IEC 60112
Descriptive Properties Value Comments
Ball Pressure Test, 75°C +/- 2°C PASSES
IEC 60695-10-2