Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® CH6310 PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® CH6310 PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CH6310 is a high heat, high flow PC/ABS resin, with nonbrominated, nonchlorinated flame retardant system. All color available.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength, Yield 61.0 MPa
8850 psi
SABIC - Japan Method
Elongation at Break 220 %
220 %
SABIC - Japan Method
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 5.10 J/cm
9.55 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 60.0 - 80.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
33.3 - 44.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 0.46 MPa (66 psi) 127 °C

@Thickness 3.20 mm
261 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C

@Thickness 3.20 mm
244 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94
5VB

@Thickness 2.00 mm
5VB

@Thickness 0.0787 in
UL 94