Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific)

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Cycoloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact, extrusion grade polycarbonate/ABS alloy.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm

@Thickness 3.20 mm
0.0050 - 0.0070 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 8.5 g/10 min

@Load 5.00 kg,
Temperature 260 °C
8.5 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 55.0 MPa
7980 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 90 %
90 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 90.0 MPa
13100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.25 GPa
326 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.78 J/cm
12.7 ft-lb/in
ASTM D256
5.60 J/cm

@Temperature -40.0 °C
10.5 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 106 °C

@Thickness 3.20 mm
223 °F

@Thickness 0.126 in
unannealed; ASTM D648