SABIC CC862 High Density Polyethylene for Injection Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer SABIC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC CC862 High Density Polyethylene for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: SABIC HDPE CC862 is a high density polyethylene specially developed for still water bottle caps that meet organoleptic properties requirements. The material offers and ideal combination of rigidity, impact strength and low warpage properties.Typical Applications:Caps & Closures for the packaging of still mineral waterCaps & Closures for beverage, food and industrial packagingSpecial Features:Good organoleptic propertiesComplies with food contacts regulationsSlip agent free gradeInformation provided by SABIC.
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D1505
ESCR 100% Igepal® 3.0 hour
3.0 hour
F50; ASTM D1693B
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 62
62
ASTM D2240
Tensile Strength at Break 18.0 MPa
2610 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Strength 25.0 MPa
3630 psi
ASTM D790
Flexural Modulus 1.00 GPa
145 ksi
ASTM D790
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256