Material Notes:
Product Description: 318CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock additives. Sufficient antioxidant and Cu-inhibitor should be added to meet specific ageing requirements. For jacketing applications, addition of Carbon Black or UV stabilizer is required.Typical Applications: One-step or two-step Silane cross-linkable insulation for Low Voltage power insulation cable, Aerial bundle cable, also suitable for telecommunication and Low Voltage power cable jacketing.Information provided by SABIC.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
load density; ASTM D1505
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength at Break 18.0 MPa
2610 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Elongation at Break 555 %
555 %
ASTM D638
Elongation at Yield 17 %
17 %
ASTM D638
1% Secant Modulus 174 MPa
25200 psi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 120 °C
248 °F
Peak; SABIC Method
Electrical Properties Metric English Comments
Volume Resistivity 6.80e+17 ohm-cm
6.80e+17 ohm-cm
at 500 V; ASTM D257
Dielectric Constant 2.25

@Frequency 1000 Hz
2.25

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 37.0 kV/mm
940 kV/in
1000 V/sec; ASTM D149
Dissipation Factor 0.00070

@Frequency 1000 Hz
0.00070

@Frequency 1000 Hz
ASTM D150
Copyright © lookpolymers.com All Rights Reserved