Material Notes:
Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792-60T
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Ultimate 33.0 MPa
4790 psi
ASTM D638-61T
Elongation at Break 30 %
30 %
ASTM D638-61T
Izod Impact, Notched 2.40 J/cm
4.50 ft-lb/in
ASTM D256-56
0.640 J/cm

@Temperature -40.0 °C
1.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 152 °C
306 °F
Flow temperature, ASTM D569-59
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
ASTM D648-56