Rostone Rosite® 4030FS SMC Thermoset Polyester, 30% Glass Reinforced  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass SMC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rostone Rosite® 4030FS SMC Thermoset Polyester, 30% Glass Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: "Zero Shrink" Grade±1/4 mil shrinkage. Provides surface smoothness for uses such as auto headlamp retainers. High impact and flexural strength combined with dimensional accuracy.Information provided by Oneida-Rostone Group.
Physical Properties Metric English Comments
Density 1.88 g/cc
0.0679 lb/in³
ASTM D792
Water Absorption 0.50 %
0.50 %
24 hrs; ASTM D570
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
shrinkage
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 8.50 J/cm
15.9 ft-lb/in
ASTM D256