Rostone Rosite® 3552C BMC Thermoset Polyester, 15% Glass Reinforced  (discontinued **)

Category Polymer , Thermoset , Composite SMC , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rostone Rosite® 3552C BMC Thermoset Polyester, 15% Glass Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features: High Stability, Non-OutgassingDesigned for applications requiring excellent stability and dimensional control. Out-gassing is virtually eliminated making it ideal for systems such as optical readers where fogging of mirrors and lenses is a problem.Information provided by Oneida-Rostone Group.
Physical Properties Metric English Comments
Density 1.94 g/cc
0.0701 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
shrinkage
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 27.6 MPa
4000 psi
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Izod Impact, Notched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
0.058 inch
Electrical Properties Metric English Comments
Arc Resistance 190 sec
190 sec
ASTM D495