Ritelok RT09 Bearing Mount Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Ritelok
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ritelok RT09 Bearing Mount Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anaerobic. Low viscosity threadlocker for tight tolerances. High torque strength, Prevent corrosion, Locks solid-will not dismantle, Vibration resistant
Physical Properties Metric English Comments
Viscosity 125 cP
125 cP
Mechanical Properties Metric English Comments
Shear Strength 20.68 MPa
2999 psi
Descriptive Properties Value Comments
Maximum Gap Fill 1 mm