Ritelok PS67 Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Ritelok
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ritelok PS67 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anaerobic. Pipe sealant, standard and stainless pipes. PS67 withstands temperatures from 65°F to 400°F (55°C-200°C), dismantled using normal tools
Physical Properties Metric English Comments
Viscosity 550000 cP
550000 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Descriptive Properties Value Comments
Pressure Resistance 69 MPa