Ritelok HP69 High Pressure Sealant

Category Polymer , Adhesive , Thermoset
Manufacturer Ritelok
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ritelok HP69 High Pressure Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anaerobic. Hydraulic sealant for general purpose sealing. Instant high pressure seal, Used on small & medium pipes, Medium viscosity
Physical Properties Metric English Comments
Viscosity 500 cP
500 cP
Descriptive Properties Value Comments
Maximum Pipe 1.91 cm
Pressure Resistance 69 MPa