Ritelok EC1500 Gap Filling CA Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Ritelok
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ritelok EC1500 Gap Filling CA Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cyanoacrylate. General purpose, high viscosity adhesive. Ideal for gap filling of porous surfaces. High bond strength, High viscosity, Excellent for gap filling
Physical Properties Metric English Comments
Viscosity 1500 cP
1500 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 20.68 MPa
2999 psi
Descriptive Properties Value Comments
Maximum Gap Fill 0.2 mm