Resirene Resirene® READ 9500 Ignition Resistant Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer Resirene S.A. de C.V.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resirene Resirene® READ 9500 Ignition Resistant Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:High FlowIgnition ResistantNo Pre-drying RequiredHigh ImpactColors AvailableApplications:Injection MoldingDark ColorsTV CabinetsElectronic EquipmentInformation provided by US distributor Calsak Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
0.0030 - 0.0070 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 5.00 kg,
Temperature 200 °C
10 g/10 min

@Load 11.0 lb,
Temperature 392 °F
G; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.4 MPa
1800 psi
ASTM D638
Tensile Strength, Yield 15.2 MPa
2200 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 1.862 GPa
270.1 ksi
ASTM D638
Izod Impact, Notched 1.34 J/cm
2.51 ft-lb/in
0.125 in.; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0