Material Notes:
Resinlab™ EP1121 Black is a two part unfilled electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexible polymer. Its low viscosity allows for good wicking and penetration into components and circuitry and also gives good air release. It has very good resistance to water, acids and bases and most organic solvents. Thermal shock and cycling properties are also enhanced by its high elongation giving it the ability to absorb difference in CTE's of substrates. It was especially formulated to a 1A:1B volume mix ratio for use in side-by-side dispensing cartridges and meter/mix and dispense equipment. EP1121 Black will reach full cure at room temperature within 24 to 48 hours. Cure time can be accelerated by the application of heat after product has gelled. Times and temperatures from 1 hour at 65°C to 10 minutes at 100°C are typical for small castings (less than 50 grams).Information Provided by Resinlab L.L.C., an Ellsworth Adhesives Company.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Part B; TM R050-16
1.05 g/cc
1.05 g/cc
Mixed; TM R050-16
1.12 g/cc
1.12 g/cc
Part A; TM R050-16
Water Absorption 0.49 %

@Time 86400 sec
0.49 %

@Time 24.0 hour
TM R050-35
Viscosity 2000 cP
2000 cP
Part B, RVT, #5, 20 rpm; TM R050-12
2200 cP
2200 cP
Mixed; TM R050-12
2400 cP
2400 cP
Part A, RVT, #5, 20 rpm; TM R050-12
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
TM R050-17
Tensile Strength at Break 2.76 MPa
400 psi
TM R050-36
Tensile Strength, Ultimate 2.76 MPa
400 psi
TM R050-36
Tensile Strength, Yield 0.689 MPa
100 psi
TM R050-36
Elongation at Break 40 - 50 %
40 - 50 %
TM R050-36
Tensile Modulus 0.0138 GPa
2.00 ksi
TM R050-36
Compressive Yield Strength 5.17 MPa
750 psi
TM R050-38
Compressive Strength 51.7 MPa
7500 psi
Ultimate; TM R050-38
51.7 MPa
7500 psi
Break; TM R050-38
Compressive Modulus 0.0345 GPa
5.00 ksi
TM R050-38
Adhesive Bond Strength 6.89 MPa
1000 psi
Lap shear; 2024 T3 Al Abraded / MEK Wipe; TM R050-37
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C
33.3 µin/in-°F
Thermal Conductivity 0.140 W/m-K
0.972 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 27.0 °C
80.6 °F
TM R050-25
Electrical Properties Metric English Comments
Volume Resistivity 8.00e+14 ohm-cm
8.00e+14 ohm-cm
Dielectric Constant 4.2

@Frequency 100 Hz,
Temperature 25.0 °C
4.2

@Frequency 100 Hz,
Temperature 77.0 °F
Dielectric Strength 17.3 kV/mm
440 kV/in
Processing Properties Metric English Comments
Pot Life 60 - 90 min
60 - 90 min
Mass: 50g; TM R050-19
Descriptive Properties Value Comments
Color Black
Mix Ratio 1:1
Volume
100:85
Weight
Copyright © lookpolymers.com All Rights Reserved