Resin Technology Group UV-403 Millennium™ UV Curable Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group UV-403 Millennium™ UV Curable Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to match a variety of specific application parameters, including MIL-APPROVED. Custom designed bonding products and expert technical assistance are always available.Resin Technology Group UV-403 Millenium™ UV Curable AdhesiveHigh clarity structural, polycarbonate and PVC bonder
Physical Properties Metric English Comments
Viscosity 1000 cP
1000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Descriptive Properties Value Comments
Color White