Resin Technology Group TIGA 951 One-Part Silver Conductive Epoxy System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 951 One-Part Silver Conductive Epoxy System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cure 10 minutes at 120°CTIGA 951 is an electrically conductive, silver-filled epoxy adhesive recommended for electronic bonding and sealing applications. This one-part, smooth paste formulation of refined pure silver and epoxy develops strong, durable, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates. It can also be used for the assembly and repair of electrical modules, printed circuits, wave guides, flat cable and high frequency shields.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 2.10 g/cc
2.10 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
Shear Strength >= 10.3 MPa
>= 1500 psi
Cured 10 minutes at 120°C, Al/Al (etched)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.00020 ohm-cm
0.00020 ohm-cm
cured 10 minutes at 120°C
Processing Properties Metric English Comments
Cure Time >= 10.0 min

@Temperature 120 °C
>= 0.167 hour

@Temperature 248 °F
Descriptive Properties Value Comments
Color Silver
Viscosity Smooth paste
After mixing