Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group TIGA 159 LV-UV Low Viscosity, Quick Gel UV Initiated, Flexible Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mix ratio 2 to 1 by volume.TIGA 159 LV-UV hybrid epoxy system is a low viscosity adhesive designed for small potting applications, bonding, laminating, sealing and structural repair applications where outstanding shock and peel resistance are required. TIGA 159 LV-UV can be gelled to a tack free, non-flow state with a few seconds of exposure to moderate UV light and then fully cured at room temperature or rapidly at elevated temperatures. The fully cured system develops strong, tough, high performance bonds to metals, ceramics, phenolics, polyesters, epoxies, urethanes and many other plastics. It is a durable, electrically insulating adhesive which provides good resistance to gases, vapors, petroleum solvents, fuels, salt solutions, mild acids and alkalis.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
Viscosity 2000 cP

@Temperature 25.0 °C
2000 cP

@Temperature 77.0 °F
Of resin
7500 cP

@Temperature 25.0 °C
7500 cP

@Temperature 77.0 °F
Of hardener
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
Flexural Strength 37.9 MPa
5500 psi
Adhesive Bond Strength 22.1 MPa
3200 psi
Al/Al
Izod Impact, Notched 2.14 J/cm
4.00 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Electrical Properties Metric English Comments
Dielectric Strength 16.1 kV/mm
410 kV/in
Dissipation Factor 0.038

@Frequency 100000 Hz
0.038

@Frequency 100000 Hz
Processing Properties Metric English Comments
Pot Life 120 - 180 min

@Temperature 25.0 °C
120 - 180 min

@Temperature 77.0 °F
100 gm mass