Resin Technology Group MX-2212 High Impact, Multi-Functional, UV Curing Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group MX-2212 High Impact, Multi-Functional, UV Curing Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This multi-functional product is a rapid setting structural adhesive. UV-MX 2212 provides high impact, resilient bonds to many similar and dissimilar substrates. Multi-functional cure bonds are formed very rapidly by using activator, heat or exposure to ultraviolet light. UV-MX 2212 is a general purpose structural, multi-functional UV curing system designed for bonding, potting and sealing applications. Bonds exhibit both toughness and flexibility and perform well under stress caused by different coefficients of expansion. UV cured bonds are translucent to 1/4” thick sections, the maximum suggested UV curable bondline thickness.Applications: Metal bonding, fillet/sealing or bridging. Encapsulation/ unitizing potting laminations. Typical uses: DC motor construction, Magnet bonding, Pump motor housings, Audio speakers, Pot cure bonding, Mounting plates.Processing: Activator Cure: Bondline thickness of 0.02"; Fixture time of 20-30 seconds; 95% full strength in 1 hour; Full cure in 18 hours.Thermal Cure: Heat can be used as a secondary cure mechanism only after UV light curing for surfaces exposed to air. 1 hour at 225°F; 1/2 hour at 250°F; 15 minutes at 300°F.Information provided by Resin Technology Group.
Physical Properties Metric English Comments
Water Absorption 1.2 %
1.2 %
Cured
Viscosity 5000 cP

@Temperature 25.0 °C
5000 cP

@Temperature 77.0 °F
Standard, uncured
25000 cP

@Temperature 25.0 °C
25000 cP

@Temperature 77.0 °F
T-grade, uncured
Thickness <= 5080 microns
<= 200 mil
Cured film, activator cure
<= 6350 microns
<= 250 mil
Cured film, UV cure
Mechanical Properties Metric English Comments
Hardness, Shore D 40 - 50
40 - 50
Cured
Tensile Strength at Break 17.2 MPa
2500 psi
Cured
Elongation at Break 160 %
160 %
Cured
Shear Strength 17.2 MPa
2500 psi
Cured, lap, steel/steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Cured
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Cured
Flash Point >= 93.3 °C
>= 200 °F
Uncured
Shrinkage 7.0 %
7.0 %
Upon Cure
Electrical Properties Metric English Comments
Dielectric Strength 18.9 kV/mm
480 kV/in
Cured
Descriptive Properties Value Comments
Color Light Straw
Composition Urethane Oligomer/ (Meth) Acrylate Monomer Blend
Solubility Isopropyl Alcohol, Chlorinated solvents
Viscosity Thixo Paste
Gel