Material Notes:
EN 239-2 is an epoxy-based, medium viscosity, cationic- curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resistant, low out-gassing polymer system capable of surviving exposure up to 200°C.Processing: UV light cure: Intensity of 200 mw/cm2; Spectral output of 300 to 500 nanometers; Optimum wavelength of 375 nanometersRecommended Aurora UV light sources:Aurora 455-S 5x5 High Intensity FloodAurora 461-S 1x6 High Intensity BeamAurora 100-S Spot Light GuideInformation provided by Resin Technology Group.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
Uncured
Viscosity 6800 cP

@Temperature 25.0 °C
6800 cP

@Temperature 77.0 °F
Uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Elongation at Break 8.0 %
8.0 %
Cured
Shear Strength 41.4 MPa
6000 psi
Cured, tensile
Thermal Properties Metric English Comments
CTE, linear 50.0 - 100 µm/m-°C

@Temperature 20.0 °C
27.8 - 55.6 µin/in-°F

@Temperature 68.0 °F
Cured
Maximum Service Temperature, Air 160 °C
320 °F
Cured
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Cured
Glass Transition Temp, Tg 130 °C
266 °F
Cured
Flash Point >= 93.3 °C
>= 200 °F
Uncured
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. Specifies clear but does not quantify
Descriptive Properties Value Comments
Color Clear
Composition Epoxy
Moisture Resistance Excellent
Cured
Toxicity Low
Copyright © lookpolymers.com All Rights Reserved