Resin Technology Group DPE080697-1 Two component Potting Compound

Category Polymer , Adhesive , Thermoset
Manufacturer Resin Technology Group
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group DPE080697-1 Two component Potting Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Technology Group DPE080697-1 Two component Potting CompoundClear, 2 part, UV/Heat/Room temperature cure epoxy potting compound.
Physical Properties Metric English Comments
Viscosity 2000 cP
2000 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
2880 min

@Temperature 23.0 °C
48.0 hour

@Temperature 73.4 °F
Pot Life >= 300 min
>= 300 min
>= 300 min
>= 300 min