Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Resin Technology Group 6850FTLVDP Oxy-Bond™ Two component Potting Compound

Category Polymer , Adhesive , Thermoset
Manufacturer Resin Technology Group
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Resin Technology Group 6850FTLVDP Oxy-Bond™ Two component Potting Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Resin Technology Group 6850FTLVDP Oxy-Cast™ Two component Potting CompoundLow viscosity, 2:1 ratio, Potting compound with high thermal conductivity
Physical Properties Metric English Comments
Viscosity 8000 cP
8000 cP
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 360 - 480 min

@Temperature 23.0 °C
6.00 - 8.00 hour

@Temperature 73.4 °F
Pot Life 15 min
15 min
15 min
15 min
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved