Material Notes:
Key PropertiesExcellent balance of chemical, electrical and mechanical properties. Semi-flexible,tough system. Ease of use. ApplicationsBonds difficult-to-bond substrates and dissimilar materials including most metals, wood, plastics, rubber, urethane and concrete. Survives harsh environments, particularly moisture, harsh chemical, marine and subsea. Exceptional performance as a universal adhesive for industrial applications. Can be applied to oily surfaces. Will cure underwater. Ambient 24 hour or accelerated thermal cure.Information provided by Reltek LLC
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
A
1.42 g/cc
1.42 g/cc
B
Mechanical Properties Metric English Comments
Tensile Strength at Break 17.94 MPa
2602 psi
ASTM D638
Tensile Strength, Yield 18.73 MPa
2717 psi
ASTM D638
Elongation at Break 23.9 %
23.9 %
ASTM D638
Elongation at Yield 11.3 %
11.3 %
ASTM D638
Tangent Modulus 369.11 MPa
53535 psi
ASTM D638
Descriptive Properties Value Comments
Energy / Volume @ Break (ft-lb/cu. in) 45.38
Energy to Break (in-lb) 65.51
Energy to Peak Load (psi) 29.45
Peak Stress (psi) 2716
Strain @ peak load (%) 12.9
TEA (ft-lb/sq in) 5.37