Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Reltek BONDiT™ B-46TH Adhesive and Sealant

Category Polymer , Adhesive
Manufacturer Reltek LLC
Trade Name BONDiT™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reltek BONDiT™ B-46TH Adhesive and Sealant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key PropertiesExcellent adhesion to low surface energy plastics without primer or surface preparation. ApplicationsVery high flexibility, 500% elongation, emphasizing high tack for un-abraded substrates and plastic films, including unetched Teflon. Excellent water and oil block for cable application. Ambient or thermal cure. May be catalyzed for fast set time.Information provided by Reltek LLC
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
A
1.42 g/cc
1.42 g/cc
B
Moisture Absorption at Equilibrium <= 1.0 %
<= 1.0 %
Viscosity 7000 cP

@Temperature 25.0 °C
7000 cP

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Clear with haze/slight amber
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved