Reliance Industries Repol R019MZ Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol R019MZ Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REPOL Polypropylene R019MZ is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol R019MZ is recommended for use in blow molding & extrusion processes. It is an ideal material for making clear bottles, containers, ball pen refills, sheets, stationery items and thermoformed products. Features:Superior processing characteristicsExcellent clarity and glossGood impact strengthInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 1.9 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50mm/min; ASTM D638
Elongation at Yield 12 %
12 %
50mm/min; ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.800 J/cm

@Temperature 23.0 °C
1.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
DSC second heating; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648