Reliance Industries Repol H250FG Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol H250FG Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REPOL Polypropylene H250FG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H250FG is recommended for use in fiber spinning operations, for making multifilament yarn and staple fiber. Features: Good spinning characteristicsConsistent processability at high line speedsGood color stabilityHigh tensile propertiesInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
50mm/min; ASTM D638
Elongation at Yield 11 %
11 %
50mm/min; ASTM D638
Flexural Modulus 1.65 GPa
239 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.250 J/cm

@Temperature 23.0 °C
0.468 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648