Material Notes:
REPOL Polypropylene H080EG is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol H080EG is recommended for use in Cast Film Applications. Repol H080EG is an ideal material for textile overwraps, packaging of readymade garments, lamination films, snack food, twist wrap, grocery and general purpose packaging.Features:Consistent processability at high production ratesBetter downgaugingGood gloss and clarityGood heat seal strengthInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
50mm/min; ASTM D638
Elongation at Yield 9.0 %
9.0 %
50mm/min; ASTM D638
Flexural Modulus 1.40 GPa
203 ksi
1% secant; ASTM D790A
Izod Impact, Notched 0.390 J/cm

@Temperature 23.0 °C
0.731 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C
208 °F
ASTM D648