Reliance Industries Repol C080MT Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Reliance Industries
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Repol C080MT Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
REPOL Polypropylene C080MT is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific catalyst system. Repol C080MT is recommended for use in injection molding processes where high impact strength is required. It is an ideal material for making battery containers, automotive and industrial products. Repol C080MT contains long term heat stabilizer as required for under the hood applications in automotive.Features:Consistent processabilityLong Term Heat Stability (LTHS)Good stiffness-impact balanceInformation provided by Reliance Industries
Physical Properties Metric English Comments
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.0 MPa
3340 psi
50mm/min; ASTM D638
Elongation at Yield 7.0 %
7.0 %
50mm/min; ASTM D638
Flexural Modulus 1.25 GPa
181 ksi
1% secant; ASTM D790A
Izod Impact, Notched 1.00 J/cm

@Temperature 23.0 °C
1.87 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648