Reliance Industries Relene D16501 Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Reliance Industries
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Reliance Industries Relene D16501 Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Relene D16501 is a UV stabilized High Density Polyethylene compound with broad molecular weight distributions, suitable for producing cable duct for optic fiber and other general purpose cables. The compound offers good processing characteristics, improved melt strength and can withstand outdoor exposure of more then 12 months. Information provided by Reliance Industries
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
Oxidative Induction Time (OIT) >= 50 min
>= 50 min
ASTM D3895
Melt Flow 0.30 g/10 min

@Load 2.16 kg
0.30 g/10 min

@Load 4.76 lb
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 0.900 GPa
131 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Users viewing this material also viewed the following: